Acid Resistant Mortars
Typical Properties
| Propertiies | POLYSIL-K Potassium Silicate Based |
POLYSIL-K Sodium Silicate Based |
FURALSET Furane Resin Based |
| Working Time at 27°C ± 2°C (min) | 15 minutes | 20 minutes | 20 minutes |
| Flexural Strength at 7 days (min) | 35 kg/cm2 | 40kg/cm2 | 75kg/cm2 |
| Compressive Strength at 7 days (min) | 100kg/cm2 | 150kg/cm2 | 350kg/cm2 |
|
Bond Strength (min) |
5kg/cm2 | 5kg/cm2 | 10kg/cm2 |
|
Absorption of Tolune by wt. (max) |
18% | 18% | 1% |