Acid Resistant Mortars

Typical Properties

Propertiies POLYSIL-K
Potassium Silicate Based
POLYSIL-K
Sodium Silicate Based
FURALSET
Furane Resin Based
Working Time at 27°C ± 2°C (min) 15 minutes 20 minutes 20 minutes
Flexural Strength at 7 days (min) 35 kg/cm2 40kg/cm2 75kg/cm2
Compressive Strength at 7 days (min) 100kg/cm2 150kg/cm2 350kg/cm2

Bond Strength (min)

5kg/cm2 5kg/cm2 10kg/cm2

Absorption of Tolune by wt. (max)

18% 18% 1%